Here’s a “Before” photo of 4 of the panels for the water feature in the kiln ready to be fired. The panels will be fired to a temperature of 1400 degrees Fahrenheit / 760 degrees Celsius over a period of around 16 hours. Some of the glass will change colour as part of the firing process. We’ll post an “After” photo tomorrow.
You can find out more about the RHS Cardiff 2010 Show here